Per the standard, the finished conduit shall not show bright adherent copper deposits after one 60 second immersion in a copper sulphate solution. After a second 60 sec. dip in the solution the conduit shall not show copper deposits on more than 25% of the conduit surface.
Samples in both trade sizes showed copper deposits after the first dip, and more than 25% copper deposits after the second dip/